Casing & Tubing Mechanical Design, API TR 5C3 / ISO 10400 Biaxial Collapse Ellipse
API 5C3 Casing Biaxial Tension Collapse Derating Formula
Calculate Casing Diameter-to-Thickness Ratio (D/t), Hencky-von Mises Biaxial Yield Reduction Factor, Effective Axial-Derated Yield Ypa (psi), and Biaxial Collapse Rating Pca (psi).
Hanging 52,000 psi of buoyant string weight on L-80 casing slashes its API 5C3 external collapse rating in HALF—crushing evacuated pipe flat during swabbing or DST evacuation
Catalog Zero-Tension Collapse Ratings Pc0 (psi, e.g. 3,810 psi for 9-5/8" 40.0 lb/ft L-80 casing at D / t = 24.37) apply ONLY at the very bottom joint where axial hanging weight is zero. Higher up a deep intermediate string, buoyant hanging tension sigma_a = Faxial / Asteel (psi positive in tension) combines with external mud-minus-internal-fluid hoop compression (-sigma_theta) on the Hencky-von Mises Distortion-Energy Yield Ellipse (API TR 5C3 / ISO 10400): axial tension pre-consumes octahedral shear capacity, degrading **Effective Circumferential Yield Strength to Ypa = Y_p * (sqrt(1 - 0.75 * (sigma_a / Y_p)^2) - 0.5 * (sigma_a / Y_p)) (psi). Across yield- and plastic-collapse regimes, Biaxial Collapse Resistance Pca ~= Pc0 * (Ypa / Y_p)** (psi, exact for yield collapse and conservative first-order design check across plastic transition)—explaining why upper-middle mixed-grade joints collapse inward when drill-stem tests evacuate internal hydrostatic back-pressure.
Verify on 9.625-in, 40.0 lb/ft (t = 0.395 in) L-80 (Y_p = 80,000 psi) Intermediate Casing—Outside_Diameter D = 9.625 in (B2), Wall_Thickness t = 0.395 in (B3), Minimum_Yield Y_p = 80,000 psi (B4), Buoyant_Axial_Stress sigma_a = 18,000 psi (B5), and Nominal_Collapse Pc0 = 3,810 psi (B6): Slenderness D / t equals 24.37 (E2), Hencky-von Mises Factor equals 0.8683 (E3), Effective Biaxial Yield Ypa drops to 69,467 psi (E4), and Derated Collapse Rating Pca equals 3,308 psi (-13.2% below handbook 3,810 psi. E5).
| API 5C3 Biaxial Casing KPI (9.625" x 0.395" L-80, Yp=80,000 psi, Pc0=3,810 psi) | Formula | Verified Output |
|---|---|---|
| Slenderness Ratio (D / t) | Casing_OD_in / Wall_Thickness_t_in | 24.37 (plastic collapse regime) |
| Hencky-von Mises Biaxial Factor | SQRT(1 - 0.75 * (sa / Yp)^2) - 0.5 * (sa / Yp) | 0.8683 (0.5015 @ 52,000 psi tension) |
| Effective Hoop Yield Ypa (psi) | Nominal_Yp_psi * Hencky_VonMises_Factor | 69,467 psi (40,121 psi under heavy hang) |
| Derated Collapse Rating Pca (psi) | Zero_Tension_Pc0_psi * Hencky_Factor | 3,308 psi (1,911 psi = -50% LOSS) |
API TR 5C3 Hencky-von Mises Distortion-Energy Biaxial Collapse Formula
Validate Casing_OD D in [2.375, 30.0] in, Wall_Thickness t in [0.15, 1.50] in (with D / t > 8), Yield_Strength Y_p in [40,000, 165,000] psi, Axial_Tension sigma_a in [0, 0.90 * Y_p] psi, and Catalog_Collapse Pc0 in [500, 25,000] psi.
=LET(od_i, B2, wt_i, B3, yp_p, B4, sa_p, B5, pc_z, B6, sr_x, sa_p / yp_p, hv_f, SQRT(1 - 0.75 * (sr_x ^ 2)) - 0.5 * sr_x, IF(OR(od_i < 2.375, od_i > 30, wt_i < 0.15, wt_i > 1.5, od_i / wt_i <= 8, yp_p < 40000, yp_p > 165000, sa_p < 0, sa_p > 0.9 * yp_p, pc_z < 500, pc_z > 25000), "Invalid Casing Input", ROUND(pc_z * hv_f, 0)))Upper-String Heavy Hanging Tension (sigma_a = 52,000 psi = 65% of Yield) Collapse Halving Check
Evaluate a joint high up the 12,000-ft string carrying B5 = 52,000 psi axial tension (65% of L-80 yield): Hencky-von Mises Factor E3 plunges to 0.5015 (Ypa = 40,121 psi in E4), chopping Collapse Resistance E5 nearly in half from 3,810 down to 1,911 psi—demanding heavier 47.0 lb/ft P-110 top-section Tapered Casing Design.
=IF(ISTEXT(E5), E5, ROUND(SQRT(1 - 0.75 * ((B5 / B4) ^ 2)) - 0.5 * (B5 / B4), 4))Try the example
Use the original values or change them to test your understanding.