Arte SheetsLearn. Try. Understand.

Ferrous Metallurgy & Foundry Heat Treatment, ASTM A897 Austempered Ductile Iron (ADI)

Austempered Ductile Iron (ADI) Ms & Ausferrite Formula

Calculate Initial Matrix Martensite-Start Ms (°C), Salt-Bath Austempering Superheat Above Ms (°C), T0-Limited Enriched Austenite Carbon C_gamma (wt%), and Enriched Ms (°C).

Why 2.4% silicon in Austempered Ductile Iron blocks cementite carbides—creating carbon-stabilized ausferrite stronger than forged steel

ASTM A897 Austempered Ductile Iron (ADI) austenitizes nodular cast iron at 870–910 °C (dissolving Matrix Carbon C_0 ≈ 0.70–0.85 wt% from graphite nodules alongside Mn and Mo) and quenches into an isothermal nitrite/nitrate Salt Bath at Tbath = 260–390 °C—strictly ABOVE **Andrews Initial Martensite-Start Ms0 = 539 - 423 * C_0 - 30.4 * Mn - 7.5 * Mo (°C, Superheat Delta_T = Tbath - Ms0 > 40 °C). Because Ductile Iron’s ~2.4–2.8 wt% Silicon suppresses brittle Fe_3C cementite precipitation during Stage-I transformation, growing acicular ferrite rejects carbon INTO surrounding austenite until reaching Bhadeshia’s T_0 Carbon-Enrichment Ceiling Cgamma,T0 = (720 - Tbath) / 195 (~1.80–2.25 wt% C). That massive carbon enrichment depresses Stabilized Austenite Ms,enr = 539 - 423 * Cgamma,T0 - 30.4 * Mn - 7.5 * Mo below -200 °C—preserving tough, TRIP-toughened Ausferrite** (alphaferrite + gammaHC) all the way to Arctic service temperatures.

Verify on an ASTM A897 Grade 900-650-09 Tough Upper-Ausferrite Suspension Arm—Dissolved_Matrix_Carbon C_0 = 0.78 wt% (B2), Matrix_Manganese Mn = 0.36 wt% (B3), Molybdenum Mo = 0.24 wt% (B4), and Isothermal_Salt_Bath Tbath = 360.0 °C (B5): Initial Ms0 equals 196.3 °C (E2), Salt-Bath Superheat Above Ms0 equals 163.7 °C (E3), T_0-Enriched Austenite Carbon reaches 1.846 wt% (E4), depressing Stabilized Ms,enr to -254.7 °C (E5).

ASTM A897 ADI Ausferrite KPI (C0=0.78%, Mn=0.36%, Mo=0.24%, Tbath=360 vs 285 °C)FormulaVerified Output
Initial Matrix Ms0 (°C)539 - 423*C0 - 30.4*Mn - 7.5*Mo196.3 °C
Salt-Bath Superheat Above Ms0 (°C)Salt_Bath_Temp_C - Initial_Ms0_C163.7 °C (88.7 °C @ lower-ADI 285 °C)
T0 Enriched Austenite C_gamma (wt%)(720 - Salt_Bath_Temp_C) / 1951.846 wt% (2.231 wt% @ 285 °C Grade 1400)
Stabilized Ausferrite Ms_enr (°C)539 - 423*C_gamma - 30.4*Mn - 7.5*Mo-254.7 °C (-417.4 °C cryogenic stability)

Andrews Martensite-Start & Bhadeshia T0 Carbon-Enriched Ausferrite Formula

Validate Matrix_Carbon C_0 in [0.50, 1.10] wt%, Mn in [0.10, 1.20] wt%, Mo in [0.00, 1.00] wt%, and isothermal Salt_Bath Tbath in [240, 420] °C strictly above Ms0 + 25 °C.

=LET(cz_w, B2, mn_w, B3, mo_w, B4, tb_c, B5, ms_z, 539 - 423 * cz_w - 30.4 * mn_w - 7.5 * mo_w, cg_w, (720 - tb_c) / 195, ms_e, 539 - 423 * cg_w - 30.4 * mn_w - 7.5 * mo_w, IF(OR(cz_w < 0.5, cz_w > 1.1, mn_w < 0.1, mn_w > 1.2, mo_w < 0, mo_w > 1, tb_c < 240, tb_c > 420, tb_c <= ms_z + 25), "Invalid ADI Schedule", ROUND(ms_e, 1)))

Wear-Resistant Grade 1400 Lower-Ausferrite 285 °C Salt Bath Check (Set Salt Bath B5 = 285 °C)

Lower the isothermal salt bath from 360 °C to 285 °C (B5 = 285) for ultra-hard mining gear teeth: Superheat E3 narrows to 88.7 °C (nucleating nanoscale acicular ferrite laths), T_0 Carbon Enrichment E4 rises to 2.231 wt%, and Stabilized Ms,enr E5 plunges to -417.4 °C.

=IF(ISTEXT(E5), E5, ROUND((720 - B5) / 195, 3))

Try the example

Use the original values or change them to test your understanding.

Further reading