Polymer Film & Flexible Packaging, Tubular Blown-Film Extrusion BUR, Layflat & DDR
Blown-Film Extrusion BUR, Layflat & Draw-Down Formula
Calculate Transverse Blow-Up Ratio BUR = D_bubble/D_die, Collapsed Nip Layflat Width (mm), Machine-Direction Draw-Down Ratio DDR, and Forming Orientation Ratio DDR/BUR.
Stretch a blown-film bubble too hard in the haul-off nip without enough Blow-Up Ratio and the bag splits lengthwise like string cheese
Tubular Blown-Film Extrusion inflates molten LLDPE / LDPE / HDPE exiting an Annular Die of Diameter Ddie (mm) and Lip Gap tdie (mm) with internal bubble air up to Frost-Line Bubble Diameter Dbubble (mm) while Overhead Nip Rolls pull the collapsed tube upward down to Target Film Gauge tfilm (um). Biaxial polymer chain orientation—and therefore dart-drop impact toughness (ASTM D1709) vs Elmendorf tear resistance—is governed by TWO orthogonal stretch ratios: Transverse Hoop Blow-Up Ratio BUR = Dbubble / Ddie (typically 2.2–3.2 for LLDPE, setting **Collapsed Layflat Width LFW = (PI() / 2) * Dbubble mm) and Machine-Direction Draw-Down Ratio DDR = (tdie * 1,000) / (tfilm * BUR). Keeping Forming Balance Ratio DDR / BUR** modest prevents hyper-aligned axial chains that tear effortlessly along the machine direction.
Verify on a 200 mm Annular LLDPE Stretch-Hood Blown-Film Tower—Annular_Die_Diameter Ddie = 200 mm (B2), Die_Lip_Gap tdie = 1.80 mm (B3), Inflated_Bubble_Diameter Dbubble = 560 mm (B4), and Target_Single-Wall_Film_Gauge tfilm = 35.0 um (B5): Blow-Up Ratio BUR equals 2.80 (E2), Collapsed Layflat Width equals 879.6 mm (E3), Draw-Down Ratio DDR equals 18.37 (E4), and Forming Orientation Ratio DDR / BUR balances at 6.56 (E5).
| TAPPI Blown-Film Tower KPI (Die D=200 mm, Gap=1.80 mm: Balanced 560mm/35um vs Narrow 320mm/20um) | Formula | Verified Output |
|---|---|---|
| Transverse Blow-Up Ratio BUR | Bubble_Diam_mm / Die_Diam_mm | 2.80 (1.60 under-blown @ 320 mm) |
| Collapsed Layflat Width LFW (mm) | (PI() / 2) * Bubble_Diam_mm | 879.6 mm (502.7 mm @ 320 mm) |
| Machine Draw-Down Ratio DDR | (Die_Gap_mm * 1000) / (Film_um * BUR) | 18.37 (56.25 excessive axial draw) |
| Orientation Balance (DDR / BUR) | Draw_Down_Ratio_DDR / Blow_Up_Ratio_BUR | 6.56 (35.16 splitty MD tear failure) |
Tubular Blown-Film Biaxial Stretch Ratios (BUR, Layflat & DDR) Formula
Validate Die_Diam Ddie > 20 mm, Lip_Gap tdie in [0.3, 5.0] mm, Bubble_Diam Dbubble >= Ddie, and Film_Gauge tfilm in [5, 500] um.
=LET(dd_m, B2, tg_m, B3, db_m, B4, tf_u, B5, bu_r, db_m / dd_m, dd_r, (tg_m * 1000) / (tf_u * bu_r), IF(OR(dd_m <= 20, tg_m < 0.3, tg_m > 5, db_m < dd_m, tf_u < 5, tf_u > 500), "Invalid Blown-Film Input", ROUND(dd_r / bu_r, 2)))Under-Inflated 1.6 BUR Thin-Gauge (320 mm Bubble, 20 um Film) MD Splitting Check
Run a narrow 320 mm bubble (BUR = 1.60 in E2) on the wide 1.80 mm LLDPE die gap while drawing down to 20 um film (B4 = 320, B5 = 20): DDR E4 rockets to 56.25 and DDR / BUR E5 jumps 5.4x to 35.16—over-aligning polyethylene lamellae axially so bags zipper-split down the machine direction.
=IF(ISTEXT(E5), E5, LET(bu_r, B4 / B2, ROUND((B3 * 1000) / (B5 * bu_r), 2)))Try the example
Use the original values or change them to test your understanding.