Extractive Metallurgy & Precious-Metals Recovery, Electrolytic Copper Refining Tankhouse
Copper Electrorefining Anode Cycle, Scrap & Slime Formula
Calculate Dissolvable Anode Copper Mass (kg), Faraday Daily Cathode Plating Rate (kg/d), Anode Campaign Life Before Scrap Pull (days), and Au/Ag/Se Anode Slime Yield (kg/anode).
Pushing copper electrorefining current density to 410 A/m² passivates impure anodes with CuSO4·5H2O crust—forcing 19% anode scrap recycle back to the anode furnace
Unlike copper *electrowinning* (insoluble Pb-Sn-Ca anodes evolving O2 at ~2.0 V), Electrolytic Copper Refining (99.5% fire-refined blister/anode copper -> 99.99% LME Grade-A ISA/Kidd stainless-blank cathodes at just 0.28–0.35 V cell voltage) electrochemically dissolves cast Copper Anodes (Mass Man kg) while leaving 12%–16% Undissolved Anode Scrap (sscr %) so lug ears never snap and drop 50 kg plates through polymer-concrete tankhouse floors. By Faraday’s Law (MCu = 63.546 g/mol, n = 2, F = 96,485.332 C/mol) across Two-Sided Active Blank Area A (m²), Current Density j (A/m²), and Cathode Current Efficiency eta_c (%), **Daily Copper Plating Rate equals mday = ((A * j) * 86,400 * 63.546 * (eta_c / 100)) / (2 * 96,485.332 * 1,000) (kg/d), fixing Total Anode Life tan = (Man * (1 - sscr / 100)) / mday (days, typically two 9–10-day cathode pulls per 18–21-day anode cycle), while insoluble Gold, Silver, Platinum, Selenium & Lead Sulfate (Rslime kg/t dissolved) settle to cell sumps as high-value Anode Slime**.
Verify on a Modern ISA-Process Tankhouse Electrolytic Cell—Cast_Anode_Mass Man = 380 kg (B2), Target_Anode_Scrap sscr = 14.0% (B3), Two-Face_Cathode_Area A = 2.05 m² (B4), Current_Density j = 310 A/m² (B5), Current_Efficiency eta_c = 96.5% (B6), and Specific_Slime_Fall Rslime = 5.80 kg/t dissolved (B7): Dissolvable Anode Copper equals 326.8 kg (E2), Daily Cathode Gain equals 17.45 kg/d (E3), Total Anode Residence Cycle equals 18.73 days (two 9.36-day ~163 kg cathode pulls. E4), and Precious-Metal Bearing Slime Yield equals 1.895 kg per anode (E5).
| Copper Electrorefining Cell KPI (380 kg Anode, A=2.05 m², Slime=5.8 kg/t) | Formula | Verified Output |
|---|---|---|
| Dissolvable Anode Mass (kg) | Cast_Anode_kg * (1 - Anode_Scrap_Pct / 100) | 326.8 kg (307.8 kg @ 19% scrap) |
| Faraday Cathode Gain (kg/d) | ((Area * j) * 86400 * 63.546 * Eff) / (2 * F * 1000) | 17.45 kg/d (22.00 kg/d @ 410 A/m²) |
| Anode Residence Life (days) | Dissolvable_Mass_kg / Daily_Cathode_kg_d | 18.73 d (13.99 d two-pull schedule) |
| Au/Ag/Pb Slime per Anode (kg) | (Dissolvable_Mass_kg / 1000) * Slime_kg_t | 1.895 kg/anode Doré feed |
Faraday Copper Electrorefining Anode Cycle, Scrap Margin & Slime Balance Formula
Validate Anode_Mass in [150, 600] kg, Anode_Scrap in [8, 35]%, Cathode_Area in [1.0, 3.6] m², Current_Density in [150, 480] A/m², Current_Efficiency in [80, 99.8]%, and Slime_Rate in [0.5, 30] kg/t.
=LET(ma_k, B2, sc_p, B3, ac_m, B4, cd_j, B5, ce_p, B6, sl_r, B7, md_k, ma_k * (1 - sc_p / 100), IF(OR(ma_k < 150, ma_k > 600, sc_p < 8, sc_p > 35, ac_m < 1, ac_m > 3.6, cd_j < 150, cd_j > 480, ce_p < 80, ce_p > 99.8, sl_r < 0.5, sl_r > 30), "Invalid Refining Input", ROUND((md_k / 1000) * sl_r, 3)))High-Intensity Overdrive (j = 410 A/m², Scrap = 19%, Eff = 92%) Nodulation & Passivation Check
Push rectifier density to B5 = 410 A/m² on high-nickel/antimony anodes where sulfate passivation forces B3 = 19.0% scrap pull and dendritic short-circuits drop efficiency to B6 = 92.0%: Daily Plating E3 rises to 22.00 kg/d, compressing Anode Replacement Cycle E4 to 13.99 days (+34% crane-handling congestion and anode-furnace remelt fuel) while Slime Capture E5 drops to 1.785 kg/anode.
=IF(ISTEXT(E5), E5, LET(md_k, B2 * (1 - B3 / 100), kd_d, ((B4 * B5) * 86400 * 63.546 * (B6 / 100)) / (2 * 96485.332 * 1000), ROUND(md_k / kd_d, 2)))Try the example
Use the original values or change them to test your understanding.