Arte SheetsLearn. Try. Understand.

LTCC Microelectronics, Glass Frits & SLS Polymer Powders, Yakov Frenkel (1945) Viscous Sintering

Frenkel Viscous Sintering Neck Ratio & Shrinkage Formula

Calculate Viscous Capillary Characteristic Time (min), Frenkel Neck-to-Particle Radius Ratio (x/r), Isotropic Linear Shrinkage (-dL/L0 %), and Frenkel-vs-Mackenzie Regime Status.

Raising LTCC glass-frit firing temperature just +35°C drops viscosity 5x (log10 eta from 8.8 to 8.1) while halving particle size—speeding densification shrinkage 10-fold

Unlike crystalline metal powders that sinter slowly by solid-state grain-boundary diffusion ((x / r)^6 ~ t), amorphous Borosilicate Glass Frits, Low-Temperature Co-Fired Ceramics (LTCC), Optical Preforms, and Selective-Laser-Sintered (SLS) Amorphous Polymers densify by Newtonian Viscous Flow Driven by Surface Tension gamma (N/m). Balancing capillary surface-area reduction against viscous dissipation across spherical particles of Radius r (um = r * 10⁻⁶ m) at Newtonian Viscosity eta = 10^(log10 eta) (Pa·s), Yakov Frenkel (1945) derived **Characteristic Capillary Time tau_v = ((eta * r) / gamma) / 60 (min), Dimensionless Neck Growth x / r = sqrt((3 * gamma * t) / (2 * eta * r)), and Early-Stage Isotropic Linear Shrinkage -Delta_L / L_0 = ((3 * gamma * t) / (8 * eta * r)) * 100%** (= 25% * (x / r)^2). Once x / r exceeds ~0.45, intersecting necks pinch open channels into isolated spherical pores governed by Mackenzie-Shuttleworth (1949) Late-Stage Pore Closure.

Verify on an LTCC Dielectric Glass-Ceramic Tape Firing Hold—Surface_Tension gamma = 0.32 N/m (B2), Particle_Radius r = 12.0 um (B3), Log10_Viscosity log10(eta) = 8.80 [Pa·s] (B4, 6.31 x 10⁸ Pa·s near Littleton softening), and Isothermal_Soak t = 24.0 min (B5): Viscous Characteristic Time equals 394.3 min (E2), Frenkel Neck Ratio x / r reaches 0.302 (E3), Linear Firing Shrinkage equals 2.28% (E4), confirming "INITIAL FRENKEL NECK STAGE" (x / r <= 0.45 in E5).

Frenkel (1945) Viscous Sintering KPI (gamma=0.32 N/m)FormulaVerified Output
Viscous Characteristic Time (min)(((10 ^ LogEta) * (r_um * 1e-6)) / gamma) / 60394.3 min (39.3 min @ fine hot frit)
Frenkel Neck Ratio (x / r)SQRT((3 * gamma * t_s) / (2 * eta * r_m))0.302 (0.756 coalesced spheres)
Isotropic Linear Shrinkage (%)((3 * gamma * t_s) / (8 * eta * r_m)) * 1002.28% (14.30% full densification)
Sintering Kinetics Regime GateIF(x_over_r <= 0.45, "INITIAL FRENKEL...", "LATE MACKENZIE...")INITIAL FRENKEL NECK STAGE

Yakov Frenkel (1945) Viscous Capillary Neck Coalescence & Linear Shrinkage Formula

Validate Surface_Tension gamma in [0.05, 1.50] N/m (~0.03–0.05 polymers to 0.30–0.40 silicate glasses), Particle_Radius r in [0.2, 500] um, Log10_Viscosity in [5.0, 13.0] Pa·s, and Hold_Time in (0, 1,440] min.

=LET(gm_n, B2, rp_u, B3, lg_v, B4, tm_m, B5, IF(OR(gm_n < 0.05, gm_n > 1.5, rp_u < 0.2, rp_u > 500, lg_v < 5, lg_v > 13, tm_m <= 0, tm_m > 1440), "Invalid Sinter Input", ROUND((((10 ^ lg_v) * (rp_u * 0.000001)) / gm_n) / 60, 1)))

Jet-Milled Fine Frit (r = 6 um) + Hotter Peak (log10 eta = 8.1, 15 min) Pore-Closure Check

Mill glass frit finer (B3 = 6.0 um) and raise peak furnace zone +35°C (B4 = 8.10 -> eta = 1.26 x 10⁸ Pa·s) for just B5 = 15.0 min: Characteristic Time E2 drops 10x to 39.3 min, driving x / r E3 to 0.756, Linear Shrinkage E4 to 14.30%, and transitioning E5 into "LATE MACKENZIE PORE CLOSURE" (where trapped N2 gas bubbles halt final 2% porosity unless fired under vacuum or He/O2).

=IF(ISTEXT(E2), E2, ROUND(SQRT((3 * B2 * (B5 * 60)) / (2 * (10 ^ B4) * (B3 * 0.000001))), 3))

Try the example

Use the original values or change them to test your understanding.

Further reading