Aerospace & EV Battery Tray Solid-State Joining, Friction Stir Welding (FSW) Energetics
Friction Stir Welding (FSW) Pitch, Heat Index & Power Formula
Calculate FSW Advance-per-Revolution Weld Pitch (mm/rev), Arbegast Pseudo-Heat Index, Mechanical Spindle Stir Power (kW), and Net Linear Heat Input (J/mm).
Fusion-weld 2xxx/7xxx aircraft aluminum and hot-cracking ruins the seam—Friction Stir Welding plasticizes metal 100 °C BELOW its melting point
Friction Stir Welding (FSW, AWS D17.3) plunges a non-consumable shouldered H13/MP159 tool rotating at N (RPM) into aluminum rocket propellant tanks and EV battery extrusion trays, traversing along the butt joint at v (mm/min) under Measured Spindle Torque M (N·m) and Thermal Transfer Efficiency eta (~0.85–0.92). Defect-free dynamic recrystallization inside the stir nugget balances two kinematic invariants: Revolution Pitch (Advance per Revolution) APR = v / N (mm/rev—too high >0.8 mm/rev starves plastic flow into internal wormhole tunnel voids; too low <0.18 mm/rev churns excess ribbon flash) and **Arbegast Pseudo-Heat Index HI = N^2 / (v * 1,000) (RPM²/(m/min)), while torque directly measures Mechanical Spindle Power P_m = (2 * PI() * N * M) / 60,000 (kW) and Net Linear Heat Input Qlin = (eta * P_m * 1,000) / (v / 60)** (J/mm).
Verify on a 6 mm AA6061-T6 EV Cooling-Plate Butt Joint—Spindle_Speed N = 950 RPM (B2), Traverse_Feed v = 380 mm/min (B3), Measured_Spindle_Torque M = 44.0 N·m (B4), and Workpiece_Thermal_Efficiency eta = 0.88 (B5): Advance-per-Revolution equals 0.400 mm/rev (E2), Pseudo-Heat Index equals 2.375 (E3), Spindle Power draws 4.38 kW (E4), and Net Linear Heat Input equals 608.2 J/mm (E5).
| AWS D17.3 Friction Stir Welding KPI (M=44 N·m, eta=0.88: Optimal 950/380 vs Over-Hot 1400/220) | Formula | Verified Output |
|---|---|---|
| Advance per Revolution APR (mm/rev) | Traverse_Speed_mm_min / Spindle_RPM | 0.400 mm/rev (0.157 mm/rev flash @ 1400/220) |
| Arbegast Pseudo-Heat Index | (Spindle_RPM ^ 2) / (Traverse_mm_min * 1000) | 2.375 (8.909 HAZ over-aging @ 1400/220) |
| Mechanical Spindle Power (kW) | (2 * PI() * Spindle_RPM * Torque_Nm) / 60000 | 4.38 kW (6.45 kW @ 1,400 RPM) |
| Net Linear Heat Input (J/mm) | (eta * Power_kW * 1000) / (Traverse_mm_min / 60) | 608.2 J/mm (1,548.2 J/mm = 2.5x HAZ softening) |
FSW Kinematic Pitch, Arbegast Heat Index & Torque-Based Linear Heat Formula
Validate Spindle_RPM in [100, 4,000], Traverse v in [20, 3,000] mm/min, Torque M > 1 N·m, and Thermal_Efficiency eta in [0.50, 0.98].
=LET(nr_p, B2, vt_m, B3, mt_n, B4, et_h, B5, pk_w, (2 * PI() * nr_p * mt_n) / 60000, IF(OR(nr_p < 100, nr_p > 4000, vt_m < 20, vt_m > 3000, mt_n <= 1, et_h < 0.5, et_h > 0.98), "Invalid FSW Schedule", ROUND((et_h * pk_w * 1000) / (vt_m / 60), 1)))Over-Hot 1,400 RPM / 220 mm/min Schedule T6 Precipitate Over-Aging Check
Spin up to 1,400 RPM while slowing feed to 220 mm/min (B2 = 1400, B3 = 220): Pitch E2 plunges to 0.157 mm/rev (extruding heavy shoulder flash), Heat Index E3 jumps 3.75x to 8.909, and Linear Heat Input E5 surges 2.55x to 1,548.2 J/mm—dissolving strengthening Mg_2Si precipitates across the Thermo-Mechanically Affected Zone (TMAZ).
=IF(ISTEXT(E5), E5, ROUND((2 * PI() * B2 * B4) / 60000, 2))Try the example
Use the original values or change them to test your understanding.