Semiconductor PVD & Thin-Film Vacuum Coating, Magnetron Sputtering Rate & Cosine Throw
Magnetron Sputtering PVD Deposition Rate & Throw Formula
Calculate Total Sputtered Atom Emission Rate (10¹⁹ atoms/s), Knudsen Cosine Wafer-Center Flux (10¹⁶ atoms/cm²·s), Film Deposition Rate (nm/min), and 500 nm Seed Coat Time (min).
Raise a magnetron wafer chuck from 8.5 to 14.0 cm to improve uniformity and inverse-square cosine throw slashes PVD deposition rate by 63%
DC and RF Planar Magnetron Sputtering (PVD) traps electrons in a race-track E x B plasma to bombard a high-purity metal target with Ar⁺ ions at Target Current I (A, Ion Arrival Rate I / e where e = 1.60217663 * 10^{-19} C). Each 400–600 eV Ar⁺ impact ejects Sputter Yield Y target atoms/ion (Y ≈ 1.8–2.3 for Cu/Ag, ~0.5–0.8 for Ti/W), emitting **dot_N = (I / e) * Y (atoms/s) in a Knudsen Cosine Angular Distribution (J ~ cos(theta)). In ballistic high vacuum (P ~ 2–5 mTorr, negligible gas scattering), Wafer-Centerline Atomic Flux at Throw Distance h (cm) equals J_s = dot_N / (PI() * h^2) (atoms/(cm²·s)), growing a solid film of Molar Mass M (g/mol) and Bulk Density rho (g/cm³) at Rdep = J_s * (M / (rho * N_A)) * 10^7 * 60** (nm/min, N_A = 6.02214076 * 10^{23} mol⁻¹).
Verify on a Copper Seed-Layer DC Magnetron Cathode—Target_Discharge_Current I = 0.85 A (B2), Ar⁺->Cu Sputter_Yield Y = 1.85 atoms/ion (B3 -> Total Ejected Flux = 0.981 * 10^{19} atoms/s in E2), Target-to-Substrate_Throw h = 8.50 cm (B4), Copper_Atomic_Weight M = 63.546 g/mol (B5), and Copper_Density rho = 8.96 g/cm³ (B6): Wafer-Center Flux hits 4.32 * 10^{16} atoms/(cm²·s) (E3), Film Growth Rate reaches 305.5 nm/min (E4), depositing a 500 nm electroplating seed layer in 1.64 min (E5).
| DC Magnetron Copper PVD KPI (I=0.85 A, Y=1.85, Cu M=63.546, h=8.5 vs 14.0 cm) | Formula | Verified Output |
|---|---|---|
| Ejected Atom Rate (x10¹⁹ atoms/s) | ((Current_A / 1.60217663e-19) * Yield) / 1e19 | 0.981 x 10¹⁹ atoms/s |
| Wafer-Center Flux (x10¹⁶ /cm²·s) | (Ejected_Atoms_s / (PI() * h_cm^2)) / 1e16 | 4.32 (1.59 @ long-throw h=14.0 cm) |
| Film Deposition Rate (nm/min) | Js * (M / (rho * 6.02214076e23)) * 6e8 | 305.5 nm/min (112.6 nm/min @ 14.0 cm) |
| Time for 500 nm Seed Layer (min) | 500 / Deposition_Rate_nm_min | 1.64 min (4.44 min cycle @ 14.0 cm) |
Sputter Yield, Knudsen Cosine Throw Flux & Thin-Film Growth Rate Formula
Validate Target_Current I > 0.02 A, Sputter_Yield Y in (0.05, 8.0], Throw_Distance h in [2.0, 50.0] cm, Atomic_Weight M in [6, 250] g/mol, and Film_Density rho in [1.5, 23.0] g/cm³.
=LET(ic_a, B2, sy_a, B3, ht_c, B4, mw_g, B5, rf_g, B6, nd_s, (ic_a / 0.000000000000000000160217663) * sy_a, js_c, nd_s / (PI() * (ht_c ^ 2)), rd_n, js_c * (mw_g / (rf_g * 602214076000000000000000)) * 600000000, IF(OR(ic_a <= 0.02, sy_a <= 0.05, sy_a > 8, ht_c < 2, ht_c > 50, mw_g < 6, mw_g > 250, rf_g < 1.5, rf_g > 23), "Invalid PVD Input", ROUND(500 / rd_n, 2)))Long-Throw 14.0 cm High-Aspect Trench Collimation Rate Penalty Check (Set Throw Distance B4 = 14.0 cm)
Retract the substrate pedestal to Long-Throw h B4 = 14.0 cm to collimate bottom coverage inside TSV vias: (8.5 / 14.0)^2 = 0.369 cuts Wafer Flux E3 to 1.59 * 10^{16} atoms/(cm²·s) and Deposition Rate E4 to 112.6 nm/min—stretching 500 nm seed coat time E5 to 4.44 min.
=IF(ISTEXT(E5), E5, LET(nd_s, (B2 / 0.000000000000000000160217663) * B3, js_c, nd_s / (PI() * (B4 ^ 2)), ROUND(js_c * (B5 / (B6 * 602214076000000000000000)) * 600000000, 1)))Try the example
Use the original values or change them to test your understanding.