Additive Manufacturing & Photopolymer 3D Printing, SLA Jacobs Working Curve Cure Depth
Stereolithography (SLA) Jacobs Cure Depth & Overcure Formula
Calculate Gaussian Centerline Peak UV Exposure Emax (mJ/cm²), Jacobs Beer-Lambert Cure Depth Cd (um), Interlayer Stitching Overcure Cd - z (um), and Cured Line Width (um).
Double an SLA galvo scan speed to halve print time and logarithmic cure depth drops BELOW the 100 um layer slice—peeling layers apart mid-print
Laser Stereolithography (SLA) sweeps a 355/405 nm Gaussian UV beam of Power P_L (mW), 1/e² Beam Radius w_0 (mm), and Galvo Scan Speed v_s (mm/s) across a liquid Photopolymer Resin Tray characterized by TWO Beer-Lambert constants: Optical Penetration Depth D_p (um, 1/e UV attenuation depth controlled by photoinitiator + UV blocker) and Critical Gelation Exposure E_c (mJ/cm²). Paul F. Jacobs derived the foundational SLA Working Curve Equations: **Peak Centerline Exposure Emax = P_L / (SQRT(PI() / 2) * (w_0 / 10) * (v_s / 10)) (mJ/cm²), Logarithmic Cure Depth C_d = D_p * LN(Emax / E_c) (um), Interlayer Stitching Overcure Delta_C = C_d - zlayer (um—MUST stay +40 to +80 um positive so green polymer chains covalently cross-link into the previous layer), and Parabolic Cured Line Width L_w = (w_0 * 1,000) * SQRT(2 * LN(Emax / E_c))** (um).
Verify on a 355 nm Industrial Ceramic/Engineering-Resin SLA Printer—UV_Laser_Power P_L = 120.0 mW (B2), Gaussian_Spot_Radius w_0 = 0.11 mm (220 um spot diameter, B3), Galvo_Scan_Speed v_s = 2,400 mm/s (B4), Resin_Penetration_Depth D_p = 145.0 um (B5), Critical_Exposure E_c = 11.5 mJ/cm² (B6), and Z-Stage_Layer_Slice z = 100.0 um (B7): Peak Exposure hits 36.27 mJ/cm² (E2), Cure Depth reaches 166.5 um (E3), Interlayer Stitching Overcure locks in +66.5 um (E4), and Cured Track Width equals 166.7 um (E5).
| Jacobs SLA Working Curve KPI (P=120 mW, w0=0.11 mm, Dp=145 um, Ec=11.5, z=100 um) | Formula | Verified Output |
|---|---|---|
| Peak Centerline Exposure Emax (mJ/cm²) | P_mW / (SQRT(PI()/2) * (w0/10) * (vs/10)) | 36.27 mJ/cm² (18.13 @ fast 4,800 mm/s) |
| Beer-Lambert Cure Depth Cd (um) | Dp_um * LN(Emax_mJ_cm2 / Ec_mJ_cm2) | 166.5 um (66.0 um < 100 um @ 4,800 mm/s) |
| Interlayer Stitching Overcure (um) | Cure_Depth_Cd_um - Layer_Slice_z_um | +66.5 um (-34.0 um DELAMINATION GAP) |
| Gaussian Cured Line Width Lw (um) | (w0_mm * 1000) * SQRT(2 * LN(Emax / Ec)) | 166.7 um (105.0 um @ 4,800 mm/s) |
Jacobs Gaussian Beer-Lambert Cure Depth, Overcure & Cured Track Width Formula
Validate Power P_L > 1 mW, Beam_Radius w_0 in [0.01, 1.0] mm, Scan_Speed v_s > 10 mm/s, Penetration D_p > 10 um, Critical_Exposure E_c > 0.5 mJ/cm², Layer_Slice z > 10 um, and above-gelation Emax > E_c.
=LET(pl_m, B2, wz_m, B3, vs_m, B4, dp_u, B5, ec_m, B6, zl_u, B7, em_x, pl_m / (SQRT(PI() / 2) * (wz_m / 10) * (vs_m / 10)), IF(OR(pl_m <= 1, wz_m < 0.01, wz_m > 1, vs_m <= 10, dp_u <= 10, ec_m <= 0.5, zl_u <= 10, em_x <= ec_m), "Invalid SLA Exposure", ROUND((wz_m * 1000) * SQRT(2 * LN(em_x / ec_m)), 1)))Doubled 4,800 mm/s Galvo Speed Negative-Overcure Delamination Check (Set Scan Speed B4 = 4,800 mm/s)
Double galvo scan speed to v_s B4 = 4,800 mm/s in "draft mode" without boosting laser mW: Emax E2 halves to 18.13 mJ/cm², Cure Depth E3 plunges to 66.0 um (< 100 um Z-step), and Overcure E4 turns negative (-34.0 um)—leaving 34 um of uncured liquid resin between every slice so cured skins float loose across the resin tray.
=IF(ISTEXT(E5), E5, LET(em_x, B2 / (SQRT(PI() / 2) * (B3 / 10) * (B4 / 10)), ROUND(B5 * LN(em_x / B6) - B7, 1)))Try the example
Use the original values or change them to test your understanding.