Arte SheetsLearn. Try. Understand.

ASME VIII Div. 3 High-Pressure Vessels & Diesel Rails, Thick-Cylinder Autofrettage

Thick-Cylinder Autofrettage & Residual Bore Stress Formula

Calculate Wall Radius Ratio K (b/a), Tresca Bore Yield-Onset Pressure Py (MPa), Autofrettage Overpressure Paf (MPa), and Elastic-Unloading Residual Bore Hoop Stress (MPa).

Pre-yielding a high-pressure diesel common-rail bore to c = 31 mm locks in -693 MPa of crack-closing compressive hoop stress—unless K > 2.22 triggers Bauschinger reverse yielding

Without pre-stressing, a thick-walled forged cylinder (Inner Bore Radius a mm, Outer Radius b mm -> Wall Ratio K = b / a, Alloy Yield Strength sigma_y MPa) begins yielding at its inner bore as soon as internal pressure hits **Tresca Elastic Limit P_y = (sigma_y / 2) * (1 - (1 / K^2))** (MPa, never exceeding 0.5 * sigma_y no matter how thick you forge the wall). ASME Section VIII Division 3 Autofrettage deliberately pumps hydraulic oil or pulls an oversize carbide swage to **Autofrettage Pressure Paf = (sigma_y / 2) * (1 - (c / b)^2 + 2 * ln(c / a)) (MPa), expanding a plastic core out to Elastic-Plastic Junction Radius c (a <= c <= b) while the outer elastic shell (c -> b) squeezes back upon depressurization. Subtracting full Lamé unloading from loaded bore stress (sigma_y - Paf) leaves Compressive Residual Bore Hoop Stress sigmatheta,res = sigma_y - Paf * ((2 * K^2) / (K^2 - 1))** (MPa)—clamp-shutting cyclic fatigue micro-cracks on 250 MPa diesel fuel rails, 300 MPa LDPE autoclave tubes, and 400 MPa waterjet intensifiers.

Verify on a 4340 Martensitic Steel High-Pressure Intensifier Barrel—Inner_Bore a = 20.0 mm (B2), Outer_Radius b = 42.0 mm (B3), Target_Plastic_Front c = 31.0 mm (B4), and Yield_Strength sigma_y = 960 MPa (B5): Wall Ratio K equals 2.10 (<= 2.22 elastic-unloading limit. E2), Initial Bore Yield Pressure P_y equals 371.2 MPa (E3), Required Autofrettage Pressure Paf equals 639.2 MPa (E4), locking in -693.4 MPa of protective compressive bore hoop stress upon unloading (E5).

ASME VIII Div. 3 Tresca Autofrettage KPI (a=20 mm, Sy=960 MPa)FormulaVerified Output
Cylinder Wall Ratio K (b / a)Outer_Radius_b_mm / Inner_Bore_a_mm2.10 (2.60 > 2.22 thick-wall regime)
Initial Bore Yield Py (MPa)(Yield_Sy / 2) * (1 - (1 / (K ^ 2)))371.2 MPa (409.0 MPa)
Autofrettage Pressure Paf (MPa)(Sy / 2) * (1 - (c/b)^2 + 2 * LN(c/a))639.2 MPa @ c=31 mm (904.0 MPa @ c=46 mm)
Elastic Residual Bore Hoop (MPa)Sy - Paf * ((2 * K^2) / (K^2 - 1))-693.4 MPa SAFE (-1,161.8 < -960 REVERSE YIELD)

Hill / Tresca Elastic-Plastic Autofrettage Pressure & Residual Hoop Formula

Validate Inner_Radius a in [2, 500] mm, Outer_Radius b in (1.2 * a, 5.0 * a], Plastic_Radius c in [a, b], and Yield_Strength sigma_y in [150, 2,200] MPa.

=LET(ra_m, B2, rb_m, B3, rc_m, B4, sy_m, B5, kw_r, rb_m / ra_m, pf_m, (sy_m / 2) * (1 - ((rc_m / rb_m) ^ 2) + 2 * LN(rc_m / ra_m)), IF(OR(ra_m < 2, ra_m > 500, rb_m <= 1.2 * ra_m, rb_m > 5 * ra_m, rc_m < ra_m, rc_m > rb_m, sy_m < 150, sy_m > 2200), "Invalid Autofrettage Input", ROUND(sy_m - pf_m * ((2 * (kw_r ^ 2)) / ((kw_r ^ 2) - 1)), 1)))

Over-Thick Wall (b = 52 mm -> K = 2.60 > 2.22, c = 46 mm) Bauschinger Reverse-Yield Check

Thicken the forging to B3 = 52.0 mm (K = 2.60 in E2) and over-autofrettage out to B4 = 46.0 mm (Paf E4 = 904.0 MPa): Purely elastic unloading predicts -1,161.8 MPa in E5—exceeding -sigma_y = -960 MPa compressive yield (and firing even earlier around -650 MPa due to the Bauschinger effect), proving why ASME KD-5 caps useful residual compression above K = 2.22.

=IF(ISTEXT(E5), E5, ROUND((B5 / 2) * (1 - ((B4 / B3) ^ 2) + 2 * LN(B4 / B2)), 1))

Try the example

Use the original values or change them to test your understanding.

Further reading